Guest
I have a few querys about welding 3/8 monel and inconel
In recent events I have been seeing welds from contractors
splitting down the seams of our cones and vapor lines. I also am seeing failure at what seems to be the heat affected
weld area. These materials are holding raw brine for a salt evaporation process and was wondering if buttering the root
joint would help or what about pre and post heat treatment.
I should mention that mig and stick welding are the foremost
process used , but what about tig welding? This is a highly
corrosive enviroment and it seems to me that a number of things need to change here. I would appreciate your opinions.
In recent events I have been seeing welds from contractors
splitting down the seams of our cones and vapor lines. I also am seeing failure at what seems to be the heat affected
weld area. These materials are holding raw brine for a salt evaporation process and was wondering if buttering the root
joint would help or what about pre and post heat treatment.
I should mention that mig and stick welding are the foremost
process used , but what about tig welding? This is a highly
corrosive enviroment and it seems to me that a number of things need to change here. I would appreciate your opinions.