1
- #1
Nashanas
Petroleum
- Apr 23, 2021
- 54
Hello,
According to API RP 582, the ferrite test should be performed prior to PWHT. But, I was reading a research article where it was shown that a large percentage of delta ferrite desolves during PWHT (in the research findings it went down from 8% to 1.2%) if the PWHT temperature range is 950 - 1050 °C. I am talking about 304H here. So, to me it seems that if I am performing PWHT in this temperature range, I should logically perform ferrite test after PWHT, as my concern should be the ferrite remaining in the final structure.
Why then is the API code insisting on perfroming ferrite test before PWHT?
According to API RP 582, the ferrite test should be performed prior to PWHT. But, I was reading a research article where it was shown that a large percentage of delta ferrite desolves during PWHT (in the research findings it went down from 8% to 1.2%) if the PWHT temperature range is 950 - 1050 °C. I am talking about 304H here. So, to me it seems that if I am performing PWHT in this temperature range, I should logically perform ferrite test after PWHT, as my concern should be the ferrite remaining in the final structure.
Why then is the API code insisting on perfroming ferrite test before PWHT?