hi,
we are casting plain carbon grades in our continuous cating machine with 0,17-0,20 % C; 0,70-0,80 % Mn; 0,15-0,20 % Si; 0,030 % S; 0,010 % P. No Aluminium and Calcium wire addition is applied in ladle furnaces. Only 30 kg of Aluminium is added during EAF tapping.
During open casting, we do not have any probem of castability in tundish zirconia nozzles. However, when we apply ladle shroud between ladle and tundsh, clogging starts in our 18 mm zirconia nozzles. Even, we have very low Aluminium and Calcium content in our steel (0,003 % Al; 0,0005), analyze of clogging matrix shows alumina. We are searching the reason.
we are casting plain carbon grades in our continuous cating machine with 0,17-0,20 % C; 0,70-0,80 % Mn; 0,15-0,20 % Si; 0,030 % S; 0,010 % P. No Aluminium and Calcium wire addition is applied in ladle furnaces. Only 30 kg of Aluminium is added during EAF tapping.
During open casting, we do not have any probem of castability in tundish zirconia nozzles. However, when we apply ladle shroud between ladle and tundsh, clogging starts in our 18 mm zirconia nozzles. Even, we have very low Aluminium and Calcium content in our steel (0,003 % Al; 0,0005), analyze of clogging matrix shows alumina. We are searching the reason.