Respected community members, I have one (only?) problem with my powder processing system and I hope someone will be willing to share his/her knowledge/experience. Here it is:
Experimentsl reactor is 12" ID, 3 ft long (with a cone at the end) and filter/fan downstream. Powder is fed from the top of the reactor into a flame (burner mounted on the top). Particles generated are 0.5-1 micron. After running the system for 1/2 an hour, most of the powder is deposited on the walls of the reactor instead of being conveyed. Gas velocity is enough to keep particles entrained but why they are sticking to the wall? Reactor T is 500 C, gas flow rate 350 slpm.
Would decreasing ID/length help and how much? Or injecting air along the walls (sweeping)?
Thanks
Experimentsl reactor is 12" ID, 3 ft long (with a cone at the end) and filter/fan downstream. Powder is fed from the top of the reactor into a flame (burner mounted on the top). Particles generated are 0.5-1 micron. After running the system for 1/2 an hour, most of the powder is deposited on the walls of the reactor instead of being conveyed. Gas velocity is enough to keep particles entrained but why they are sticking to the wall? Reactor T is 500 C, gas flow rate 350 slpm.
Would decreasing ID/length help and how much? Or injecting air along the walls (sweeping)?
Thanks