spud22
Structural
- Apr 7, 2003
- 17
We are considering installing a condensing economizer on a NG fired boiler which will also be fired with 10% biogas. Concern is H2S, with approximately 400 ppm H2S in condensate. Materials proposed are 304 SS tubes and 1100 Al fins. Is this a proper application, or do we need to go to 304 or 316 SS fins and/or tubes?