PhilEduard
Mechanical
- Aug 24, 2004
- 36
All,
Power piping does not consider weld srength reduction factor W (Wc in Caesar II) but process pipng does and B31.3 addresses a situation where at temp. more than 1500 deg F., W should be obtain by the Designers themselves. Does anyone knows where this figure would come normally?
Thanks Guys,
Phil
Power piping does not consider weld srength reduction factor W (Wc in Caesar II) but process pipng does and B31.3 addresses a situation where at temp. more than 1500 deg F., W should be obtain by the Designers themselves. Does anyone knows where this figure would come normally?
Thanks Guys,
Phil