Olcay
Mechanical
- Jul 11, 2001
- 3
Situation:
We are heat treating a part made of sheet metal 50CrV4 used as clamp. There is a test for stress corrosion as : Put the parts under stress, in a 0,9% HCl solution, and they must stand at least 8 minutes
before broken.
Problem:
We could not solve which parameters of hardening and tempering process will effect the results of this test.
We are heat treating a part made of sheet metal 50CrV4 used as clamp. There is a test for stress corrosion as : Put the parts under stress, in a 0,9% HCl solution, and they must stand at least 8 minutes
before broken.
Problem:
We could not solve which parameters of hardening and tempering process will effect the results of this test.