millimillenary
Materials
- Apr 21, 2010
- 3
P2 etch (ferrous sulfate, sulfuric acid, DI water, 160F, 25 minutes) is needed on aluminum at my facility prior to application of a structural primer paint on the aluminum. This is fine on wrought aerospace alloys like 2024, 6061, 7075. Today we tried an alloy similar to an A356 aluminum casting alloy, except this alloy has up to 10 wt% silicon. This time, the P2 etch created a brown/black residue on the alloy in question.
Does anyone know what is happening here? Can anyone recommend an etching process or solution (preferably to a MIL standard or ASTM or such)? Should I be doing FPL etch instead?
Thanks,
Patrick
Does anyone know what is happening here? Can anyone recommend an etching process or solution (preferably to a MIL standard or ASTM or such)? Should I be doing FPL etch instead?