Is there anyone of you who can suggest of how I will weld for the third time a snap differential axle shaft of my pick up. I have bought that converted pick up from somewhere and only found out that they cut short the differential to narrow the track on the rear, not original one. Shaft was cut halfway and welded. Understood that twisting force cause it to break.
What I did before was to have it repaired 2 times on a nearby shop. As I have seen it, they make a 40 deg total (more or less) V cut on both ends of shaft, welded and trued again. I have doubt that they did not used specified welding rods suitable for shaft material. Is post heat treatment necessary? Your suggestions are very much appreciated.
Merry X'mas,
Cengrtecs
Is there anyone of you who can suggest of how I will weld for the third time a snap differential axle shaft of my pick up. I have bought that converted pick up from somewhere and only found out that they cut short the differential to narrow the track on the rear, not original one. Shaft was cut halfway and welded. Understood that twisting force cause it to break.
What I did before was to have it repaired 2 times on a nearby shop. As I have seen it, they make a 40 deg total (more or less) V cut on both ends of shaft, welded and trued again. I have doubt that they did not used specified welding rods suitable for shaft material. Is post heat treatment necessary? Your suggestions are very much appreciated.
Merry X'mas,
Cengrtecs