We have been asked to produce a bearing ring from Silicon Resin Bonded Fabric with a strengthining Aluminium sheet bonded to one side(simple). But! the rings hve to pass a 500 hour test of imersion in Skydrol hydralic oil at 130 deg C, the adhesives used so far have not lasted 100 hrs before delaminating (not simple). Can anyone suggest a possible adhesive?
Thanks
We have been asked to produce a bearing ring from Silicon Resin Bonded Fabric with a strengthining Aluminium sheet bonded to one side(simple). But! the rings hve to pass a 500 hour test of imersion in Skydrol hydralic oil at 130 deg C, the adhesives used so far have not lasted 100 hrs before delaminating (not simple). Can anyone suggest a possible adhesive?