We have purchased 2 test rings.
1. ASTM A105
2. ASTM A350LF2
On the mill certificate, the vendor mentioned the same heat number for the two materials.
My question:
Is it possible that the 2 materials can be prepared from the same heat ?
Thanks in advance.
1. ASTM A105
2. ASTM A350LF2
On the mill certificate, the vendor mentioned the same heat number for the two materials.
My question:
Is it possible that the 2 materials can be prepared from the same heat ?