Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

ASME BPVC sec IX welding procedure

Status
Not open for further replies.

millimeters

Petroleum
Jul 19, 2013
21
I appreciate your thoughts on this.

We need a ASME sec IX welding procedure to cover welding P1G1,2,3 to P1G1,2,3. I want to cover up to 1 inch wall thickness. Proven impact property ir required. I noticed companies are using two PQR welding dual rated 516 Gr60/70 to group 3 plate in 0.249 and 0.5 inch thickness to cover range.

-What is dual rated 516 60/70? Material list of ASME sec IX does not have dual rated material.
-Any idea on number of PQR and how to proceed on this?
 
Replies continue below

Recommended for you

Assuming the weld filler metal is the same, you will need qualify 4 impact test coupons.
 