hi,
Currently I'm developing 2 procedures. 1 is 625 overlay on Stainless steel 410 and the other is a closure joint of 410 to 410.
May I know what's the hardness requirement as per NACE? I could never seem to get the hardness as per NACE requirement of maximum 250 HV10.
For F6Nm, there's a paper that says that the maximum allowable hardness is at 275HV10. Since 410 is also martensitic stainless steel like F6Nm, can I use the maximum allowable as 275HV10?
Currently I'm developing 2 procedures. 1 is 625 overlay on Stainless steel 410 and the other is a closure joint of 410 to 410.
May I know what's the hardness requirement as per NACE? I could never seem to get the hardness as per NACE requirement of maximum 250 HV10.
For F6Nm, there's a paper that says that the maximum allowable hardness is at 275HV10. Since 410 is also martensitic stainless steel like F6Nm, can I use the maximum allowable as 275HV10?