I'm using it to support and preserve integrity after local impacts, currently i'm using carbon fiber with epoxy resin, but i'm having troubles with localizing the damage zone after impact. It feels that the epoxy is too brittle and after impact it cracks all ove and i get voids all over and...
hi to all
I would like to make a thin 0.25-0.37" laminate with high flexability
could some one recommend Graphite fiber with elastomeric reisen.
I would like to process it about 220-280 F so it will fit my current process as well.