there is a specific reason why for relay application of both ferritic SS or Si-Fe alloys, Br and Hc values are generally required misuring at the maximum flux density of 1 Tesla ( 10kG) instead of saturation flux density Bs ?
During these last years, I found that there is a lot of different opinions about the use of "improved or enhanced machinabilty of austentic stainless steels according to Nace MRO175-2009. I'm talking to standard Astm 304/304L and 316/316L and NOT to free machining stainless steel as Astm 303.In...