Hi,
I need to know the formula for calculating deflection of corrugated (concentrically) diaphragms under application of pressure. If I am not mistaken, this formula is obtained by modifying the deflection formula for flat diaphragms, wherein the effect of corrugation is taken care by...
Hi,
I need to know the bursting pressure of both laminated glass (100mmOD,3mm thk) and Toughened glass (100mmOD,3mm thk).
Do I need to do the test myself and find out or would this information be available with glass manufacturers / reference books etc.
Thanks in advance.
Pras
Hi,
I need following info on the bourdon tube manufacturing :
What kind of heat treatment should be given after tube bending, if the materials are as follows :
(I) SS316
(II)CuSn8 (Werkstoff-Nr. 2.1030 DIN 17662)
(III)CuZn15 (Werkstoff-Nr. 2.0240)
Thanks in advance.
Pras
Hi,
I am looking for a good book or website where technical information on pressure gauges like types, materials, design criteria etc would be available.
Could anyone help me out on this please.
thanks in advance.
pras
Hi,
I need to use the JIS flanges in materials equivalent to ASTM A182F316L/ASTM A351 CF3M and ASTM A182 F316 / ASTM A351 CF8M. Hence would like to know the following :-
(1) Relevant JIS standard for pressure temperature ratings
(2) Relavant JIS standard for material details (for stainless...
Hello,
Does anybody know if following materials are chemically compatible with Hexene CH3(CH2)3CH=CH2 in the temperature range of 40°C to 200°C.
(1) Titanium (ASTM B348 gr 2)
(2) ASTM A351 gr CF3M
(3) Inconel 718 rings(with nickel coating)
I have not been able to get this medium in chemical...
NOTE :- SAME POST IS REPEATED IN 'CORROSION ENGINEERING'
Pras (Mechanical) Aug 9, 2002
Hi,
We are facing failure problems of a springs made up of SS316L material ( 1.0 mm wire diamter, 6.3mm outer diamter, 9.5mm length)which are used in our special pipe fittings. The spring is exposed to the...
Hi,
We are facing failure problems of a springs made up of SS316L material ( 1.0 mm wire diamter, 6.3mm outer diamter, 9.5mm length)which are used in our special pipe fittings. The spring is exposed to the fluid and supposed to work in 'compressed condition'. It is clear from our observations...
Hi,
I am planning to use a ceramic component (Alumina 99.7%) for one of my projects. I need to test the following of the same :-
(1) Composition :- Though the supplier claims that the alumina content is 99.7%, I would like to know the best method to test the same.
(2) Hardness (Wear...
Hello,
I need to offer products made in stainless steel grades F316L(ASTM A182), CF3M(ASTM A351)and CF8M(ASTM A351) for one of the off-shore projects. The fluid used is water having following contents :
Ion symbol concentration in mg/l
Sodium Na+ 30,390
calcium Ca2+ 9,383
Magnesium...
Hello,
I am in process of designing a flanged meter housing of Class 1500 rating at design temperature of 464°F in CF3M material. The flanges to be used are of material A182 F316L. The inner radius of the housing is 39 mm ( 1.5354”). I have followed following procedure to determine the minimum...
In one of the applications, we need to fit stainless steel (SS304 grade)threaded caps on a transmitter housing made up of aluminium alloy (GD AlZn10Si8Mg). The transmitter housing is meant for housing electronic modules and expected to withstand temp upto 75 degC. The housing is not expected to...
Hi,
We need to coat the stainless steel springs with teflon (25-30 microns)in order to increase the corrosion resistance. The spring wire diamter is 0.55mm and its un-compressed length is 9.5mm. We tried a few times but failed to achieve the continuous teflon coating all round the spring wire...