Dear all members,
Hydrophobis membrane usually must be prewetted. And in every book or journal I have read, they always use ethanol.
I am confuse. Why must ethanol?
Why not methanol instead?
Thank you,
Yul
I am doing a research with polysulphone membranes. The pretreatment for the membranes was done by submerged it in the ethanol 80%. As far as I know, after submerged in the ethanol, the flux should be going up. But my experiment result showed that the flux was going down. Can anybody please help...