Have you seen this kind of failure before if you do not follow the instruction below?
Kerem.
"All austenitic stainless steel surfaces proposed to be insulated and having temperature above 50C shall be suitably protected by wrapping with aluminium foil 0.1mm thick or painted with suitable...
Actually I am dealing with a software much more focussed on isometric pipeline drawings with pre-defined pipeline materials in various standards.
Kerem.
Sulfuric acid is pumped from a day tank at normal conditions.
No special heating or cooling.
The discharge pressure of the pump is 3 bar.
Monel will be used both in discharge and suction.
Kerem.
We are planning to use Monel 400 for two different sulfuric acid lines of which concentrations are %5 and %95. What do you think the corrosion resistance performance of Monel will be?
Better than 316SS, same or worse?
Kerem.