Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Recent content by Fibre and resin guy

  1. Fibre and resin guy

    Influence of post-cure temperature on final properties

    Hello Compositepro, Thanks for your insight, I think I understand a bit better what happens. My initial undertsanding was that as long as you were above Tg (in the liquid or sol/gel state), molecular mobiltity was sufficient to have decent crosslinking kinetics. This is what can be found in...
  2. Fibre and resin guy

    Influence of post-cure temperature on final properties

    Hello all, I am not coming from a chemical background so there is a phenomenon for which I cannot find a decent explanation. I currently use thermoset polyurethane retort adhesives and coatings. These products have a fairly low fully reacted Tg (somewhere between 0 and 10°C) to remain flexible...
  3. Fibre and resin guy

    Twist-off type threads design and manufacturing

    Hello, I'd like to find a clever way to clamp a two parts insert for a composite plate with a hole during bonding, with minimal rotation to keep the two parts roughly aligned (for cosmetic reasons) even if plate thickness varies slightly.
  4. Fibre and resin guy

    Twist-off type threads design and manufacturing

    Thanks, that's a starting point ! Apparently there is a german standard too, but most of the info I find relates to the overall dimensions rather than the thread profile/pitch.
  5. Fibre and resin guy

    Twist-off type threads design and manufacturing

    Hello all, I am looking for some references (handbooks, tutorials, etc) related to the design of twist-off type threads, similar to those that can be found on jar lids for instance. I suspect these are partial threads with a very high pitch, but would be happy to have some advice or rulle of...
  6. Fibre and resin guy

    Design allowable value knockdown for wet layup

    Hello Waldemar, Wet lay-up Carbon Epoxy is still fairly used for marine structures. with our without vacuum bagging. ISO 12115-5:2008 (and maybe later revisions ?) has tables and calculations for determining design allowables for such materials, based on fibre mass or volume content depending on...