A106B has higher Si, though I do not think there is a nondestructive technique (portable fluorescence or spectroscopic PMI devices) that can differentiate. If you have NACE Refin*Cor database, there may be some data on Hydrogen Induced Damage of pipe. I believe I know of only one case reported...